Applying the MicroMetal
Using a Microcement Trowel, work your way out from one corner creating a random edge pattern. Keep trowel movements small and random, avoid long sweeping arches – as these will show through to your final finish.
Use the grain in the liquid metal as your level – if you apply it thicker than the size of the grain, the finish won’t be as strong and will require a lot more sanding. Run the trowel back over each section that you have put down to smooth it out and remove excess product.
Run your finger or a corner trowel along internal corners to push the microcement into the corner and then gently trowel away the excess product.
Cemher Iron Micrometal + Metal Resin
| Oxidising the Metal | Polishing the Metal | |
|---|---|---|
| Process | Oxidising the Metal: Apply 1 coat of liquid metal & oxidise | Polishing the Metal: Apply 2 coat of liquid metal & polish |
| Mix Ratio | Oxidising the Metal: 5kg Metal Powder : 500ml - 1l Metal Resin | Polishing the Metal: 5kg Metal Powder : 500ml - 1l Aquatix |
| Standard Consumption | Oxidising the Metal: 5kg per 10m2 | Polishing the Metal: 10kg per 10m2 |
| Estimated Drying Time |
Oxidising the Metal:
Before Accelerator: Minimum 30 minutes No Maximum Before Sealers: Minimum 24 hours No Maximum |
Polishing the Metal:
Between Coats: Minimum 30 minutes No Maximum Before Polishing: Minimum 24 hours No Maximum |
| Tools Required |
Oxidising the Metal:
Microcement Trowel Microcement Mixer PPE |
Polishing the Metal:
Microcement Trowel Microcement Mixer PPE |
Cemher Copper Micrometal + Metal Resin
| Oxidising the Metal | Polishing the Metal | |
|---|---|---|
| Process | Oxidising the Metal: Apply 1 coat of liquid metal & oxidise | Polishing the Metal: Apply 2 coat of liquid metal & polish |
| Mix Ratio | Oxidising the Metal: 5kg Metal Powder : 500ml - 1l Metal Resin | Polishing the Metal: 5kg Metal Powder : 500ml - 1l Aquatix |
| Standard Consumption | Oxidising the Metal: 5kg per 10m2 | Polishing the Metal: 10kg per 10m2 |
| Estimated Drying Time |
Oxidising the Metal:
Before Accelerator: Minimum 30 minutes No Maximum Before Sealers: Minimum 24 hours No Maximum |
Polishing the Metal:
Between Coats: Minimum 30 minutes No Maximum Before Polishing: Minimum 24 hours No Maximum |
| Tools Required |
Oxidising the Metal:
Microcement Trowel Microcement Mixer PPE |
Polishing the Metal:
Microcement Trowel Microcement Mixer PPE |
Cemher Bronze Micrometal + Metal Resin
| Oxidising the Metal | Polishing the Metal | |
|---|---|---|
| Process | Oxidising the Metal: Apply 1 coat of liquid metal & oxidise | Polishing the Metal: Apply 2 coat of liquid metal & polish |
| Mix Ratio | Oxidising the Metal: 5kg Metal Powder : 500ml - 1l Metal Resin | Polishing the Metal: 5kg Metal Powder : 500ml - 1l Aquatix |
| Standard Consumption | Oxidising the Metal: 5kg per 10m2 | Polishing the Metal: 10kg per 10m2 |
| Estimated Drying Time |
Oxidising the Metal:
Before Accelerator: Minimum 30 minutes No Maximum Before Sealers: Minimum 24 hours No Maximum |
Polishing the Metal:
Between Coats: Minimum 30 minutes No Maximum Before Polishing: Minimum 24 hours No Maximum |
| Tools Required |
Oxidising the Metal:
Microcement Trowel Microcement Mixer PPE |
Polishing the Metal:
Microcement Trowel Microcement Mixer PPE |